News

Technological visit to factories for testing fur velour recipes.
29.08.2025
In the fur direction, recipes using chemicals "SN-Sh1", "SN-MF", "SN-N-9", "Fermentol 23" and the enzyme "Dowellzym FA" were tested on the article of fur velour. After drying and pre-finishing before dyeing, the leather tissue and hairline were not greased. In the finished form, uniform dyeing was obtained in terms of hair height and skin area. The fat content in the leather tissue was normal. The work of the chemicals was positively evaluated....
Technological visit to the tannery for testing dyeing-fatliquoring and finishing recipes.
25.08.2025
The company Shebekinskaya industrialnaya khimiya, LLC has conducted a technological visit to the tannery to test dyeing-fatliquoring and finishing recipes. As part of the technological trials, the following have been tested: • dyeing-fatliquoring recipe of split-suede, which had positive feedback; • coloured dyes, new fat liquors "SMH-479", "SMH-500", which were positively evaluated by the tannery's managers; • finishing recipes: full and corrected grain nappa, corrected grain floater, Pull-up article, "Clouds" article using chemicals from Shebekinskaya industrialnaya khimiya, LLC (Russia) and Dowell (China); • urethane for top coating “Ekotop-1” and “Ekotop-2”. They were positively evaluated. Their high gloss and excellent resistance to wet rubbing were noted....

Testing recipes at the fur factory.

17-07-2024

         The company Shebekinskaya  industrialnaya  khimiya, LLC has tested the following recipes and chemicals at one of the fur factories:

1.Cleaning and degreasing processes with products "SN-SK" and "SN-SPK" on fur and wool sheepskin were carried out. The chemicals worked well, the factory technician noted a positive result.

2. In dyeing of the articles "Fur lining" and "Suede sheepskin", the fat liquor “SMH-400” was used. It was noted that the sheepskin articles obtained do not differ from factory batches in terms of the quality of purity of the leather tissue and hair.

3. A control batch of fur suede was carried out using the enzyme “Dowellzym FA” from DOWELL, (China). When summarizing the results, the factory technician noted the effect of the enzyme: the leather tissue was thinner than that of the sheepskin of the production batch.

309290, Shebekino town, Belgorod region, Rzhevskoye shosse str., 16, Floor 3,
tel.: +7(47248)3-18-10